Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.0 MPa @Temperature 23.0 °C |
3920 psi @Temperature 73.4 °F |
Y direction, Condition A; ASTM D638 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Tensile Strength, Ultimate | 27.0 MPa @Temperature 23.0 °C |
3920 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.9%); ASTM-D638 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |