Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1062 MPa @Diameter 12.7 mm, Temperature 25.0 °C |
154000 psi @Diameter 0.500 in, Temperature 77.0 °F |
Welded then age-hardened |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Ultimate | 1060 MPa @Temperature 23.0 °C |
154000 psi @Temperature 73.4 °F |
|
Special Metals NIMONIC® Alloy PE11 A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at.. |