Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 900 MPa @Temperature 23.0 °C |
131000 psi @Temperature 73.4 °F |
|
Special Metals NIMONIC® Alloy PE16 A precipitation-hardenable nickel-iron-chromium alloy with an addition of molybdenum for solid-solution strengthening. It has good strength and oxidation resistance at temperatures to about 1380°.. |
|||
Tensile Strength, Ultimate | 900 - 1050 MPa @Diameter <=100 mm |
131000 - 152000 psi @Diameter <=3.94 in |
Rm., unmachined |
Assab Steels 709M Machinery Steel ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened t.. |