Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.4 MPa

@Temperature 23.0 °C
9490 psi

@Temperature 73.4 °F
ASTM D1708
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L