Mechanical Properties Metric English Comments
Flexural Toughness 0.0524 MPa
7.60 psi
ASTM D790
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. ..