Polymer Property : Peel Strength = 40.2 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.0877 - 7.05 kN/m
0.500 - 40.2 pli
Average value: 1.46 kN/m Grade Count:353
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Peel Strength 0.0877 - 7.05 kN/m
0.500 - 40.2 pli
Average value: 1.30 kN/m Grade Count:376
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..