Polymer Property : Peel Strength = 9.90 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.74 kN/m
9.90 pli
Bond Strength; Arlon SQA-TMS-023
Arlon 28540R015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1528 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for t..
Peel Strength 1.74 kN/m
9.90 pli
PVC, 180°
3M Scotch-Weld™ 6111 Green Bulk only Adhesive
Same as 6111 tan but green in colorInformation provided by 3M
Peel Strength 1.74 kN/m
9.90 pli
Bond Strength; Arlon SQA-TMS-011
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for..
Peel Strength 1.74 kN/m
9.90 pli
PVC, 180°
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive
Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M
Peel Strength 1.74 kN/m
9.90 pli
Bond Strength; ASTM D624
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..