Polymer Property : Peel Strength = 77.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 13.5 kN/m
77.0 pli
180°, Polyacrylic, Cotton duck failed during testing
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Peel Strength 13.5 kN/m
77.0 pli
180°, Polycarbonate, Cotton duck failed during testing
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..