Mechanical Properties Metric English Comments
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9502 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9505 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9672 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9674 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 1.074 kN/m
6.125 pli
to stainless steel, 90°, 72 hr at 70°C; ASTM D3330
3M 9039 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9552 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..
Peel Strength 1.074 kN/m
6.125 pli
Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hr at RT, 4.9 mil; ASTM D3330
3M 9555 Adhesive Transfer Tapes with Adhesive 220
3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p..