Polymer Property : Peel Strength = 5.70 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.999 kN/m
5.70 pli
Copper; 1 oz. EDC post Solder Float; IPC-TM-650 2.4.8
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a..
Peel Strength 0.999 kN/m
5.70 pli
X, Y direction; after solder float 1 oz. EDC; IPC-TM-650 2.4.8
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Peel Strength 0.999 kN/m
5.70 pli
X, Y direction; after solder float 1 oz. EDC; IPC-TM-650 2.4.8
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Peel Strength 0.999 kN/m
5.70 pli
X, Y direction; after solder float 1 oz. EDC; IPC-TM-650 2.4.8
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Peel Strength 0.999 kN/m
5.70 pli
at elevated temperature; IPC-TM-650.2.4.8.2a
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy
The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free ..
Peel Strength 0.999 kN/m
5.70 pli
after exposure to process solutions; IPC-TM-650.2.4.8
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o..