Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9471 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9471 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9671 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9671 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9673 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9673 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Polyester, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7731FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | 90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330 |
3M 7993MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9471PC Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330 |
3M 9471PC Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.55877 kN/m | 3.1875 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |