Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 0.526 kN/m | >= 3.00 pli | Silicone Aluminum; Cured; ASTM D1876 |
Parker Chomerics Tecknit CON/RTV-II 2 Part Silver Filled RTV Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FL018 Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM052R Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM073 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Matte Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester ov.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM092R Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM098 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP017802 Matte White Polypropylene Label Product 3M™ Matte White Polypropylene Label Products FP010602, FP010609 and FP017802 are matte white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP021502 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
3M Scotchcal™ 50-10 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
3M Scotchcal™ 50-73 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7125-105 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7725-103 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to FRP |
3M Scotchlite™ IJ5100-10 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Permanent; Available in 15 colors, including black (which reflects whit.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to FRP |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Peel Strength | 0.526 - 0.877 kN/m | 3.00 - 5.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ IJ180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM022R Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM14J Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM14K Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM16B Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM452T Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FMV01202 Triangle Void Polyester Label Products 3M™ Triangle Void Polyester Label Products FMV01202 and FMV01402 are a tamper-indicating stock designed to provide a triangle pattern in the facestock when removal is attempted. These label product.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FMV01402 Triangle Void Polyester Label Products 3M™ Triangle Void Polyester Label Products FMV01202 and FMV01402 are a tamper-indicating stock designed to provide a triangle pattern in the facestock when removal is attempted. These label product.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FMV0E Void Polyester Label Products 3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP020601 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
3M Scotchcal™ 50-58 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7725-20 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7725-59 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM018 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |