Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 605 Transparent Film Tape Scotch® Transparent Film Tape 605 is designed for various light-duty packaging applications such as attaching, mending, gift wrapping, holding and L-Clips. This product offers good performance over.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Adhesion to Steel; ASTM D3330 |
3M 5490 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | to Steel; ASTM D3330 |
3M Scotch® 232 High Performance Masking Tape Scotch® High Performance Masking Tape 232 is designed to be used in medium temperature paint bake operations.Information provided by 3M |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.29582 kN/m | 1.6875 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |