Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.219 kN/m | 1.25 pli | to Steel; ASTM D3330 |
3M 450EK Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Finely Textured Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Finely Textured Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 356 Transparent Label Protection Tape Scotch® Label Protection Tape 356 is a transparent, tough film tape made especially for label protection in outdoor applications or where the application demands extra resistance to moisture, chemi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 3179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3179 has a very high tack adhesive system to help provide temporary protection of plastics and fabrics.Information provided by 3M |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | PP, 180° peel, 2 mil Al foil backing, 15 min dwell @ RT; ASTM D3330 |
3M 92015 Double Coated Tape with Adhesive 200MP 3M™ Double Coated Tapes with 3M™ Adhesive 200MP feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. The 3M adhesive 200MP provide.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D1000 |
3M Scotch® 35 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identif.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Backing; ASTM D1000 |
3M Scotch® 35 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identif.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | to Steel; ASTM D3330 |
3M 450XL Extended Liner Tapes 3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | Adhesion to Steel; ASTM D3330 |
3M 4F94 Fire Retardant Carpet Protective Tape 3M™ Fire Retardant Carpet Protective Tape 4F94 is a flame retardant, thicker polyethylene tape with a very high-tack adhesive system used for temporary protection of carpets during construction or .. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.219 kN/m | 1.25 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |