Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.60 - 2.40 kN/m | 9.13 - 13.7 pli | ASTM D903 |
Permabond 731 Cyanoacrylate, toughened PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Peel Strength | 1.60 - 2.40 kN/m | 9.13 - 13.7 pli | ASTM D903 |
Permabond 735 Cyanoacrylate, toughened PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Peel Strength | 1.60 - 2.40 kN/m | 9.13 - 13.7 pli | ASTM D903 |
Permabond 737 Cyanoacrylate, toughened PERMABOND® 737 is a toughened cyanoacrylate with improved impact and peel strength for maximum flexibility. Its increased temperature resistance and dark color make 737 suitable for a wide range of.. |
|||
Peel Strength | 1.80 - 2.40 kN/m | 10.3 - 13.7 pli | ISO 4578 |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |