Mechanical Properties Metric English Comments
Peel Strength 10.0 - 12.0 kN/m
57.1 - 68.5 pli
Cured for 15 mins at 200°C
Permabond ET5401 Epoxy Resin
PERMABOND® ET5401 is a two-part, 2:1 mixable, semi-flexible toughened no slump epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plastics and compo..
Peel Strength 8.00 - 12.0 kN/m
45.6 - 68.5 pli
ISO 4578
Permabond TA4202 Toughened Acrylic Adhesive
PERMABOND® TA4202 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni..
Peel Strength 0.0219 - 12.0 kN/m
0.125 - 68.5 pli
Average value: 2.82 kN/m Grade Count:38
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..