Mechanical Properties Metric English Comments
Peel Strength 2.45 kN/m
14.0 pli
Arlon AD255 Woven Glass and PTFE
Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED).
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe..
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin..
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi..
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate
Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch..
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon DiClad 880 PTFE/Woven Fiberglass Laminate
Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch..
Peel Strength 2.45 kN/m
14.0 pli
Arlon AD250 Woven Glass and PTFE
Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED).
Peel Strength 2.45 kN/m
14.0 pli
After Thermal Stress; IPC TM-650 2.4.8
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per..
Peel Strength 2.45 kN/m
14.0 pli
on canvas
3M Scotch-Weld™ 3764 Hot Melt Adhesive
Bonds variety of plastics including polycarbonate, polyethylene, and polypropylene and Flexible at low temperaturesInformation provided by 3M
Peel Strength 2.45 kN/m
14.0 pli
Polyester-Supported Vinyl, 180°, Aging 7 Day @ 140°F
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..
Peel Strength 2.45 kN/m
14.0 pli
Wood -Supported Vinyl, 180°, Aging 7 Day @ 140°F
3M Scotch-Weld™ 2262 Plastic Adhesive
Features:It is a high strength adhesive with exceptional resistance to plasticizer migration and bonds vinyl extrusions, flexible and rigid vinylsIt dries clear, is non-staining and features a very ..