Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9320 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Peel Strength | 2.312 kN/m | 13.19 pli | after thermal shock (30 sec. at 260°C); IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |