Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 13.5 kN/m | 77.0 pli | 180°, Polyacrylic, Cotton duck failed during testing |
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 13.5 kN/m | 77.0 pli | 180°, Polycarbonate, Cotton duck failed during testing |
3M Scotch-Weld™ TE100 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |