Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.9422 kN/m
5.375 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
3M 9832 Double Coated Tapes with Adhesive 300MP
3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7903 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7903FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7905 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7908 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7908FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
3M 7909 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
Peel Strength 0.9422 kN/m
5.375 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
3M 9832HL Double Coated Tapes with Adhesive 300MP
3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape..