Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.90937 kN/m | 5.1875 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polycarbonate, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330 |
3M 7620/7890 White Vinyl Label Material 3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick ta.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.90937 kN/m | 5.1875 pli | 90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330 |
3M 7959MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |