Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion |
Dielectric Polymers NT-5511-2 Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityHigh temperature resistantApplications: For automotive and other masking .. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion |
Dielectric Polymers NT-8511-2 Masking Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityHigh temperature resistantApplications: For automotive and other masking .. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to steel; ASTM D1000 |
3M 1125 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M 3381 HVAC Construction Value grade aluminum foil tape. UL 723 ClassifiedInformation provided by 3M |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Photopolymer, Adhesion; ASTM D3330 |
3M 414DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7741 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | High Surface Energy Plastic (ABS), Ultimate bond, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 966 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | >= 0.438 kN/m | >= 2.50 pli | Bond Strength |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon T2020-R004 0.020" (0.508 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide x 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone TapeDesign/Construction: Interleave: Polyethylene Product: Cured Self-Fusing Silicone RubberCross-Secti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 3771 Standard Message Box Sealing Tape Scotch® Box Sealing Tape 3771 is a standard message packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consist.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8643 Easy Open Carry Handle Tape Scotch® Easy Open Carry Handle Tape 8643 is reinforced with continuous polypropylene monofilaments in the backing that offers the unique patented advantage of providing a straight “zipper-like” e.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | Stainless Steel, Adhesion; ASTM D3330 |
3M 412DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polypropylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | 12 in/min, 90° pullback, FRP |
3M Diamond Grade™ 983 Conspicuity Markings 3M™ Diamond Grade™ Conspicuity Markings Series 983 are highly retrorflective micro-prismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The ref.. |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M P1510 Medical Permanent Acrylic Adhesives 3M™ Medical Permanent Acrylic Adhesives P1510 demonstrates excellent peel and tack performance and are designed for use in the medical attachment market.Information provided by 3M |
|||
Peel Strength | 0.438 kN/m | 2.50 pli | HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |