Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.40538 kN/m | 2.3125 pli | Adhesion to Steel; ASTM D3330 |
3M 470 Electroplating Tape 3M™ Electroplating Tape 470 is a conformable and abrasion-resistant vinyl tape with excellent resistance to most chemicals used in typical electroplating processes.Information provided by 3M |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Adhesion to Steel; ASTM D3330 |
3M 470L Electroplating Tape 3M™ Electroplating Tape 470L is a linered version of 3M vinyl tape 470 that may be used for die-cutting or large area applications.Information provided by 3M |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | to Steel; ASTM D3330 |
3M Scotch® 218 Fine Line Tape Scotch® Fine Line Tape 218 is a high-performance film backed tape with low profile and high adhesion to achieve excellent paint liens and for other masking and holding applications.Information prov.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | 90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330 |
3M 7951 Hi-Performance Acrylic 300MP This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | 90° Peel, PET/PET, Initial (20 mins); ASTM D3330 |
3M 7951 Hi-Performance Acrylic 300MP This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | 90° Peel, PET/PET, Initial (20 mins); ASTM D3330 |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | 90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330 |
3M 7961MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Adhesion to Steel; ASTM D3330 |
3M 8902 Polyester Tape 3M™ Polyester Tape 8902 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.40538 kN/m | 2.3125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |