Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.3725 kN/m | 2.125 pli | Polyester, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7733FL UV Resistant Polyester Overlaminating Film 3M™ UV Resistant Polyester Overlaminating Film 7733FL utilizes a clear polyester film that is recommended for optimum durability and superior outdoor UV exposure and print fade protection. 3M™ Adh.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polycarbonate, 180° Peel, 10 min Dwell at RT; ASTM D3330 |
3M 7811 Dot Matrix Printable Polyimide Label Material 3M™ Dot Matrix Printable Polyimide Label Material 7811 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand .. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Stainless Steel, 90° peel, 12"/min, 72 hr dwell RT; ASTM D3330 |
3M 9447 Adhesive Transfer Tape 3M™ Adhesive Transfer Tape 9447 is specifically designed for use with 3M™ Label Component Systems for protected graphics printing of polyester films. Also can be used in constructing custom tamper.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Adhesion to Steel; ASTM D3330 |
3M 528 Impact Stripping Tape 3M™ Impact Stripping Tape 528 is a thick impact stripping tape used to provide excellent surface protection during plastic media blast (PMB) paint stripping operations.Information provided by 3M |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | HD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | to Steel; ASTM D3330 |
3M Scotch® 213 High-Temperature Masking Tape Scotch® Tape 231 is a very high-temperature resistant tape for use in masking and holding applications where temperatures reach 350°F (177°C) up to 30 minutes. This tape is generally the most tra.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polyester, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7730FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.3725 kN/m | 2.125 pli | Polypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9832HL Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |