Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.33964 kN/m | 1.9375 pli | Adhesion to Steel |
3M 3334 Aluminum Foil/Scrim/PE Facing Tape 3M™ Aluminum Foil Tape 3334 has a high performance aluminum foil/bidirectional fiberglass scrim/polyethylene film laminate backing coated with a special pressure sensitive acrylic adhesive which ex.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Adhesion to Steel; ASTM D3330 |
3M 8991 Polyester Tape 3M™ Polyester Tape 8991 is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag sea.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | HD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | LD Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7603 Clear Vinyl Label Material 3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack an.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Painted Metal, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7603 Clear Vinyl Label Material 3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack an.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | ABS, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7603 Clear Vinyl Label Material 3M™ Clear Vinyl Label Material 7603 is a soft, flexible vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick tack an.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7908FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | Adhesion to Steel; ASTM D3330 |
3M 8991L Polyester Tape 3M™ Polyester Tape 8991L is a blue polyester tape with a silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag se.. |
|||
Peel Strength | 0.33964 kN/m | 1.9375 pli | 90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330 |
3M 9059MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |