Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.2849 kN/m | 1.625 pli | Adhesion |
Dielectric Polymers NT-590DL Protective Film
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized Class 392°FHigh temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications:.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Adhesion |
Dielectric Polymers NT-590-2 Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyimide film backing.Features: U.L. recognized class 392°FHigh temperature resistantClean tape removalApplications: For high temperature masking, protecting gol.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7000 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7000FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7002FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7600 Removable Vinyl Label Material 3M™ Removable Vinyl Label Material 7600 is a conformable white vinyl stock that utilizes 3M™ Adhesive 500 which offers clean removability on most surfaces for up to one year, as well as, excellent.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Adhesion to Steel; ASTM D3330 |
3M 5421 Polyethylene Tape 3M™ Polyethylene Tape 5421 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7200 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7920 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7920 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. 3M™ Adhesive .. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Adhesion to Steel; ASTM D3330 |
3M 8905 Polyester Tape 3M™ Polyester Tape 8905 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Adhesion to Steel; ASTM D3330 |
3M 8911 Polyester Tape 3M™ Polyester Tape 8911 is a transparent polyester tape with silicone adhesive that can be used in composite bonding, splicing, and applications that may require high temperature, chemical, and abr.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | to Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9019 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polypropylene, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330 |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.2849 kN/m | 1.625 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7906 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |