Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.263 kN/m | 1.50 pli | LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7047 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7732FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | LD Polypropylene, 90° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7027 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7029 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7032 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7045 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7901 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7901 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | to ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9019 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polyethylene |
3M Fastbond™ 100 Lavender Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polyethylene |
3M Fastbond™ 100 Neutral Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Adhesion to Steel; ASTM D3330 |
3M 477 Vinyl Tape 3M™ Vinyl Tape 477 is comprised of a conformable, transparent vinyl backing with a versatile rubber adhesive. It is an excellent tape to use where abrasion resistance, transparency, conformability .. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7730FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7730FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Polyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7742 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7840 Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Adhesion to Steel; ASTM D3330 |
3M 8402 Polyester Tape 3M™ Polyester Tape 8402 is a film tape with a silicone adhesive for composite bonding and splicing of many silicone coated papers and films.Information provided by 3M |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Adhesion |
Dielectric Polymers NT-581 Fume Mask
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Good conformabilityChemical resistantApplications: For protecting large areas of printed circuit boards from splash and fumes duri.. |
|||
Peel Strength | 0.263 kN/m | 1.50 pli | Adhesion |
Dielectric Polymers NT-583 Linered Polyimide Film Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityChemical resistantApplications: For PCB masking during the solder strip b.. |