Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 247 g/25 mm | 247 g/in | |
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b.. |
|||
Seal Strength | 247 g/25 mm | 247 g/in | |
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge Data provided by DuPont Packaging Polymers.An exceptionally strong polyester film designed to package foods. The film is suitable for heating food products in microwave or conventional ovens. Can b.. |