Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 1200 - 4500 g/25 mm | 1200 - 4500 g/in | Average value: 2860 g/25 mm Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Seal Strength | >= 1200 g/25 mm | >= 1200 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Seal Strength | 1200 - 1400 g/25 mm | 1200 - 1400 g/in | Average value: 1300 g/25 mm Grade Count:4 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Seal Strength | >= 1200 g/25 mm | >= 1200 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one.. |
|||
Seal Strength | 1200 g/25 mm | 1200 g/in | HDPE, bar temp 204°C |
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc.. |