Mechanical Properties Metric English Comments
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D638
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film)
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LD 103.59 Industrial Film Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin
Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a ..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LDPE LD 105.30 Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
1% Secant Modulus, TD 255 MPa
37000 psi
ASTM D882
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Copyright © lookpolymers.com All Rights Reserved