Mechanical Properties Metric English Comments
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta..
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability..
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit..
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion
Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac..
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac..
1% Secant Modulus, TD 180 MPa
26100 psi
ISO 527-3
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit..
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM-D882
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer
FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr..
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM D882
Braskem LH0820/30AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount.Applications: Lamina..
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM-D882
Braskem LL6801N LLDPE Blown Film Extrusion Polyethylene Copolymer
The LL6801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing ..
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM D882
Braskem Green PE SLH0820/30AF Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Description: SLH0820/30AF is a LLDPE hexene copolymer produced by Braskem. It offers outstanding processability combined with excellent mechanical properties. Very low gel amount. The minimum biobas..
1% Secant Modulus, TD 180 MPa
26100 psi
ASTM D882
SABIC HP2022 Series Low Density Polyethylene for Blown Film
Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:..