Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
1% Secant Modulus, TD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
1% Secant Modulus, TD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
1% Secant Modulus, TD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F.. |
|||
1% Secant Modulus, TD | 160 MPa | 23200 psi | ASTM-D882 |
Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer Braskem Flexus 9211 is a LLDPE hexene copolymer produced through a metallocene catalyst, which presents excellent impact and puncture strength beyond a differential sealing performance compared with.. |
|||
1% Secant Modulus, TD | 160 MPa | 23200 psi | ASTM-D882 |
Braskem LL3800N HDPE Cast Film Extrusion Polyethylene Copolymer The resin LL3800N is a high-density polyethylene, copolymer octene-1, produced by the solution process for the extrusion of plain films with excellent mechanical properties. It has an antirust addit.. |