Mechanical Properties Metric English Comments
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
ExxonMobil Exceed™ 1012 MJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
ExxonMobil Exceed™ 1012 MK Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymers. Films made from Exceed 1012 mVLDPE resin have outstanding cold temperature toughness, impact strength and p..
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin
Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit..
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend ..
1% Secant Modulus, TD 131 MPa
19000 psi
ASTM D882
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the..