Polymer Property : 1% Secant Modulus, TD = 170000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1170 MPa
170000 psi
ASTM D882
ExxonMobil HDPE HTA 001HD High Density Polyethylene (HMW) Resin
Product Description: HTA 001HD is a high weight HDPE film grade. Films made from HTA 001HD exhibit excellent impact and toughness properties as well as high stiffness. Availability: Africa & Middle ..
1% Secant Modulus, TD 1170 MPa
170000 psi
ASTM D882
ExxonMobil HDPE HTA 001HP2 High Density Polyethylene (HMW) Resin
Product Description: HTA 001HP2 is a high molecular weight HDPE film grade providing very good processability on high output extruders. Films made from HTA 011HP2 exhibit excellent impact and toughn..
1% Secant Modulus, TD 1170 MPa
170000 psi
ASTM D882
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin
Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can..