Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 214 MPa | 31000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | Blown Film at 1 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
(discontinued **) Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Westlake LF1040 Butene Linear Low Density Polyethylene Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120B LLDPE Blown & Cast Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip .. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | Cast Film at 1.25 mil; ASTM D-882 |
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D882 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
1% Secant Modulus, TD | 214 MPa | 31000 psi | ASTM D-882 |
Bapolene® 200B Polyethylene, Film Extrusion Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an.. |