Mechanical Properties Metric English Comments
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion)
ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake Elevate™ EF545 4% Ethylene Vinyl Acetate Copolymer
Westlake EF545 resin is a 4% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low t..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake EP413 Low Density Polyethylene
WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films ,..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films ..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
Westlake LF1020 Butene Linear Low Density Polyethylene
Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil LD 102.LC Thin Gauged Film Resin
L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and ..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin
Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin
Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil NTX™ NTX 104 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil NTX™ NTX 141 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil NTX™ NTX 150 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
1% Secant Modulus, TD 207 MPa
30000 psi
ASTM D882
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin
Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made from Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. The..