Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
Westlake EF601 Low Density Polyethylene Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1518HA Metallocene Polyethylene Resin Product Description: Exceed 1518HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.09 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
1% Secant Modulus, TD | 193 MPa | 28000 psi | ASTM D882 |
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |