Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 144 MPa | 20900 psi | ASTM D 882 |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
1% Secant Modulus, TD | 144 MPa | 20900 psi | ASTM D882 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |