Mechanical Properties Metric English Comments
1% Secant Modulus, MD 338 MPa
49000 psi
ASTM-D882
Westlake EB171 MDPE Medium Density Polyethylene
Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr..
1% Secant Modulus, MD 338 MPa
49000 psi
ASTM D882
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)
Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus..
1% Secant Modulus, MD 338 MPa
49000 psi
ASTM D882
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for L..