Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 67.6 MPa | 9810 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 310 Blown Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |
|||
1% Secant Modulus, MD | 67.6 MPa | 9800 psi | ASTM D882 |
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications Product Description: Exact 3131 is an ethylene-based hexen plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3131 is designed for both monolayer and multilayer coex.. |
|||
1% Secant Modulus, MD | 67.6 MPa | 9800 psi | ASTM D882 |
ExxonMobil EXACT™ 3139 Plastomer for Cast Film Applications Product Description: Exact 3139 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3139 is designed for both monolayer and multilayer coe.. |