Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 352 MPa | 51000 psi | ASTM D882 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |