Mechanical Properties Metric English Comments
1% Secant Modulus, MD 270 MPa
39200 psi
ASTM-D882
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional ..
1% Secant Modulus, MD 270 MPa
39200 psi
ASTM-D882
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer
Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve..