Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
Chevron Phillips MarFlex® D163 Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 312.09 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 312.23 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |
|||
1% Secant Modulus, MD | 146 MPa | 21200 psi | ASTM D882 |
ExxonMobil LD 312.82 High Impact Film Resin LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging.Information provided by ExxonMobi.. |