Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
ExxonMobil Exceed™ 1012CA Film Resin
(discontinued **) Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a.. |
|||
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
LyondellBasell Petrothene® NA442051 Low Density Polyethylene ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b.. |
|||
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, MD | 131 MPa | 19000 psi | ASTM D882 |
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |