Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 177 - 420 MPa | 25700 - 60900 psi | Average value: 331 MPa Grade Count:45 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Flexural Yield Strength | 20.0 - 420 MPa | 2900 - 60900 psi | Average value: 174 MPa Grade Count:331 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Yield Strength | 215 - 420 MPa | 31200 - 60900 psi | Average value: 320 MPa Grade Count:24 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Flexural Yield Strength | 28.3 - 420 MPa | 4100 - 60900 psi | Average value: 215 MPa Grade Count:18 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |