Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 80.0 - 270 MPa | 11600 - 39200 psi | Average value: 186 MPa Grade Count:236 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Flexural Yield Strength | 40.0 - 270 MPa @Temperature -55.0 - 275 °C |
5800 - 39200 psi @Temperature -67.0 - 527 °F |
Average value: 128 MPa Grade Count:8 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Flexural Yield Strength | 90.0 - 270 MPa | 13100 - 39200 psi | Average value: 206 MPa Grade Count:49 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |