Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 103 - 250 MPa | 15000 - 36300 psi | Average value: 172 MPa Grade Count:47 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Flexural Yield Strength | 133 - 250 MPa | 19300 - 36300 psi | Average value: 194 MPa Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Flexural Yield Strength | 109 - 250 MPa | 15800 - 36300 psi | Average value: 180 MPa Grade Count:45 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Flexural Yield Strength | 158 - 250 MPa | 22900 - 36300 psi | Average value: 192 MPa Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Yield Strength | 75.0 - 250 MPa | 10900 - 36300 psi | Average value: 141 MPa Grade Count:63 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 50.0 - 250 MPa | 7250 - 36300 psi | Average value: 117 MPa Grade Count:50 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Yield Strength | 13.8 - 250 MPa | 2000 - 36300 psi | Average value: 142 MPa Grade Count:122 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |