Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 62.1 - 108 MPa | 9010 - 15700 psi | Average value: 87.3 MPa Grade Count:52 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Flexural Yield Strength | 46.2 - 108 MPa | 6700 - 15700 psi | Average value: 88.8 MPa Grade Count:13 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Yield Strength | 39.3 - 108 MPa | 5700 - 15700 psi | Average value: 67.5 MPa Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |