Polymer Property : Flexural Yield Strength = 9950 psi
Polymer Property :
Flexural Yield Strength =
9950 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Yield Strength
68.6
MPa
9950
psi
ASTM D790
Hannam Chemical Hanalac H-2938 ABS
Flexural Yield Strength
68.6
MPa
9950
psi
ASTM D790
Hannam Chemical Hanalac HU-600 ABS