Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Spartech Royalstatâ„¢ R63 ABS/PVC Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Clariant Renol CAB1000 Cellulose Acetate Butyrate Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
PlastxWorld DAICEL STYROL® GW30 HIPS UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |